At TrueFit, quality isn’t just a standard — it’s our promise. Every patient deserves the very best that modern dentistry can offer. That’s why we rely exclusively on trusted, name-brand materials backed by decades of research and proven clinical success. With TrueFit, there are no shortcuts and no compromises — only consistent excellence in every restoration we create.
2. Flexural Strength: Tested according to ISO 6872:2015, sample size 3×4×40 mm.
3. Transparency: All light transmittance, light source D65, sample thickness 1.0 mm.
| Shade | VITA 16 Shade |
| Strength (MPa) | ≥ 1,100 MPa |
| Thickness (T/mm) | 12T, 14T, 16T, 18T, 20T, 22T, 25T |
| Diameter (Ø) | Ø95, Ø98 (Please contact us for Ø95 size) |
| Features |
• The strength of all layers are 1,100 MPa. • Multi-layer Disc more specialized for the posterior. • 5 – 4 – 9 layers. • It is easy for beginners to use by reducing the number of coloring. • Indications: – Single Anterior/Posterior, Bridge – Full arch – Implant case |

(Anterior)

(Posterior)


- Sintering Schedule
-
Step 1 Room Temperature to 900°C :
- Step 2 900°C to 1530°C :1 hour and 50 minutes (110 minutes)
- Step 3 Hold 1530°C : 2 hours (120 minutes)
- Step 4 250°C : Cooling for 3 hours and 40 minutes (220 minutes)
-
※ Total Time : 9 hours and 15 minutes.
(Based on ARUM Sintering Schedule)
2. Flexural Strength: Tested according to ISO 6872:2015, sample size 3×4×40 mm.
3. Transparency: All light transmittance, light source D65, sample thickness 1.0 mm.
| Shade | VITA 16 Shade |
| Strength (MPa) | ≥ 1,100 MPa |
| Thickness (T/mm) | 12T, 14T, 16T, 18T, 20T, 22T, 25T |
| Diameter (Ø) | Ø95, Ø98 (Please contact us for Ø95 size) |
| Features |
• The strength of all layers are 1,100 MPa. • Multi-layer Disc more specialized for the posterior. • 5 – 4 – 9 layers. • It is easy for beginners to use by reducing the number of coloring. • Indications: – Single Anterior/Posterior, Bridge – Full arch – Implant case |

(Anterior)

(Posterior)


- Sintering Schedule
-
Step 1 Room Temperature to 900°C :
- Step 2 900°C to 1530°C :1 hour and 50 minutes (110 minutes)
- Step 3 Hold 1530°C : 2 hours (120 minutes)
- Step 4 250°C : Cooling for 3 hours and 40 minutes (220 minutes)
-
※ Total Time : 9 hours and 15 minutes.
(Based on ARUM Sintering Schedule)
2. Flexural Strength: Tested according to ISO 6872:2015, sample size 3×4×40 mm.
3. Transparency: All light transmittance, light source D65, sample thickness 1.0 mm.
| Shade | VITA 16 Shade |
| Strength (MPa) | Occlusal area : 600 MPa ~ Cervical area : 1,100 MPa |
| Thickness (T/mm) | 12T, 14T, 16T, 18T, 20T, 22T, 25T |
| Diameter (Ø) | Ø95, Ø98 (Please contact us for Ø95 size) |
| Features |
• Structure of Disc by properly mixing
「4Y & 5Y」 powder. • The body under the support load is 1,100 MPa strength, and the occlusal requiring a transparent layer is 600 MPa, a Multi-Disc that reproduces both the chroma of the body and the transparency of the occlusal. • 5+4 = 9 layers • Anterior/Posterior Zirconia that anyone can easily and universally produce. • Indications: – Single, Bridge (≤ 4 Units) – Use both Anterior and Posterior |

(Anterior)

(Posterior)


(Up to 4-Unit bridge with Molar)
- Sintering Schedule
-
Step 1 Room Temperature to 900°C :
- Step 2 900°C to 1530°C :1 hour and 50 minutes (110 minutes)
- Step 3 Hold 1530°C : 2 hours (120 minutes)
- Step 4 250°C : Cooling for 3 hours and 40 minutes (220 minutes)
-
※ Total Time : 9 hours and 15 minutes.
(Based on ARUM Sintering Schedule)
2. Flexural Strength: Tested according to ISO 6872:2015, sample size 3×4×40 mm.
3. Transparency: All light transmittance, light source D65, sample thickness 1.0 mm.
| Shade | VITA 16 Shade |
| Strength (MPa) | Occlusal area : 600 MPa ~ Cervical area : 800 MPa |
| Thickness (T/mm) | 12T, 14T, 16T, 18T, 20T, 22T, 25T |
| Diameter (Ø) | Ø95, Ø98 (Please contact us for Ø95 size) |
| Features |
• Use the excellent TOSOH 「5Y」 powder to match • The color of the teeth Layered shades to fit. • 5+4 = 9 layers • Anterior aesthetic zirconia that even beginners can easily make. • Indications: – Single, Bridge (≤ 4 Units) – Only Anterior case |



(Anterior)

(Only Anterior Case)
- Sintering Schedule
-
Step 1 Room Temperature to 900°C :
- Step 2 900°C to 1530°C :1 hour and 50 minutes (110 minutes)
- Step 3 Hold 1530°C : 2 hours (120 minutes)
- Step 4 250°C : Cooling for 3 hours and 40 minutes (220 minutes)
-
※ Total Time : 9 hours and 15 minutes.
(Based on ARUM Sintering Schedule)
UTML Ultra Translucent Multi Layered
STML Super Translucent Multi Layered
HTML PLUS High Translucent Multi Layered PLUS
High Esthetic Potential for Zirconia Dental Restorations* The "KATANA™ Zirconia" UTML and STML, which feature translucency similar to natural enamel, are now available!
You can achieve a highly esthetic restoration, with predictable results, while saving time (even when fabricating esthetic anterior restorations). "Comparison with our conventional products.
Higher Translucency Than Conventional Zirconia
Our proprietary research and development has increased the translucency of "KATANA™ Zirconia" UTML more than conventional zirconia. This enables you to have natural translucency.
Wide Range of Clinical Applications Using Monolithic Restoration
You can fabricate many restorations, from esthetic anteriors to posterior bridges by selecting the right translucency and mechanical properties*
UTML Ultra Translucent Multi Layered
UTML has the most translucency among the "KATANA™ Zirconia" series, and is recommended for fabricating anterior crowns or laminate veneers. Two different shade types are available: Standard shade and Enamel shade.
STML Super Translucent Multi Layered
STML has a well-balanced combination of translucency and mechanical properties. This version of "KATANA™ Zirconia" has gradations of translucency as well as color, exhibiting a masking effect in the cervical area. Using this series, one can easily obtain the desired shades to accommodate the variety found in prepared tooth conditions of clinical cases.